SKYBON ES-AMP-403 Saturated polyester resin Trial product - 广州昊毅新材料科技股份有限公司

SK saturated polyester resin

SKYBON ES-AMP-403 Saturated polyester resin Trial product

                                      

 

performance

parameter

unit

AMP-403

AMP-501

Exterior

-

particles

flaky

molecular weight

g/mole

10,000

15,000

Viscosity

dl/g

0.45

0.56

glass transition temperature

Degree C

40

14

Softening point (℃)

Degree C

120

90

Acid value

KOH mg/g

<3

<3

OH Value

KOH mg/g

7-10

3-6

 

 

 Application

STEP

STEP

STEP

MP45

PU

(PU)+ES-AMP

CPP

MEK,EA

MEK,EA

Toluene

IPA

IPA

 

Features
      high gloss
Good compatibility with alcohols and all pigments
Excellent pigment wetting

Dissolution method
1. Put all the solvent into the reactor
2. Put the ES-AMP solid into the reactor while stirring
3. After adding all the ingredients, raise the temperature of the reactor to 90-100 degrees, stir for 2 hours, the maximum pressure of the reactor: 2kg/cm2
4. Turn off the heating system and continue stirring for one and a half hours to allow the temperature of the reactor to drop naturally.
5. Stop stirring, the solution needs to be filtered, and put the solution into a 200kg bucket